Skip to main content Skip to search Skip to main navigation

Rosegold Solution 18 Karat

Product information "Rosegold Solution 18 Karat"

Rosegold Solution from Betzmann Galvanik

This Rose Gold Brush/Pen Plating Solution (18 Karat) doesn’t have to be mixed beforehand. It can be used for both brush and pen plating. You can use either the Platinum Electrode (2.5 – 3.0 volts) or the Carbon Electrode (2.0 – 2.5 volts) with this solution.
One of the outstanding qualities of the solution is that it plates very fast compared to other brush plating solutions.
You can compare the plating rates using our online brush plating calculator on the links bar above.
 
Failure to observe the above precautions will result in the degeneration of the gold component in the solution. This will cause copper-rich plating, which will tarnish quickly.
 
Please see below for more products related to Rose Gold Brush/Pen Plating Solution (18 Karat).
Recommended electrode: Carbon, Voltage: 3 – 3.5
 
 
Gold Concentration 9.1g/l
Voltage Range (Platinum Electrode) 2.5 – 3.0 volts*
Voltage Range (Carbon Electrode) 2.0 – 2.5 volts*
Electrode Carbon
Alloy consistency (at mix ratio 1Mixer:10 K-Gold) 75% Gold, 25% Copper
Colour designation 5N
Temperature 20 – 25 °C
Plating Rate at (3.3 volts, carbon electrode) Approx. 0.5 microns per minute (max)
Hardness Hard: In excess of 250 – 300 Hv
Density of deposit 14.4 g/cm3
Stress Medium
Special storage requirements Away from sunlight
Shelf life 1-2 years (please refer to notes below)
Health and Safety classification Irritant
Special considerations None (cyanide-free)
Transport (UN number) None: Not classified as dangerous for transport

* The lower voltage range should be applied when using smaller swabs.

Notes:

  • Remove any existing layers of rose gold before plating.
  • Store in hermetically sealed container with lid firmly closed. Small
  • volumes for day-day use should be stored in a stoppered syringe.
  • Higher voltages can be used with plating rates in excess of 3 microns
    per minute (spot).
    A lower voltage range is recommended when plating above 1 micron to prevent
    dullness and subsequent polishing.

Similar Items

Carbon Electrode 6mm
Graphite round rod - Graphite rod anode - Graphite electrode for gold plating.  Graphite electrodes are ultimate for all coatings. The advantage is that in some coatings with stainless steel electrodes, the dislodged metal parts disturb the coating. This does not happen with graphite electrodes, because graphite also filters out contaminated liquids. With bath electroplating, they also need to be replaced occasionally as they slowly dissolve during the plating process.   With pad electroplating, simply loosen the screw on the handle and replace with a new one.   Diameter 6 mm, length approx. 9 cm    Features Used for Doesn’t contaminate Cleaner Activating and electro-cleaning  Its resistive properties help to heat the solution you’re plating with Chromium plating, which needs to be plated at 25 degrees celsius; its natural heating action helps to maintain the solution’s optimal temperature Low cost Can be used for all plating processes but carbon electrodes deteriorate over a period of time and discolour swabs (discolouration does not affect the plating quality)    

€5.90*
Metal Polish Ultrafine
MPU Fine is as the name implies; a fine version of our MPU. It is ideal when working on thin flash coatings of gold as it removes the minimum of metal. If further plating is required, just as with Ultra, then all you have to do is wipe well with a clean paper towel and continue plating.As the particle size is no more than the wavelength of visual light, there is no chance of leaving any scratch.The scratch-free property of MPU makes it excellent for polishing very soft surfaces such as gold and silver plate. Even the smallest solid contaminant on a swab or final polishing cloth will produce a scratch in gold and silver. MPU fine polishes these scratches out whilst protecting the properties of the plated layer.     Features Used for Fine version of MPU Working on thin flash coatings of gold as it removes the minimum amount of metal. As with MPU, if further plating is required all you have to do is wipe well with a clean paper towel and continue plating Particle size of MPU Fine no more than the wavelength of visual light No chance of leaving a scratch on even the softest of metals, such as gold or silver plate – great also for removing scratches in plastic and glass  

Content: 0.1 Liter (€125.00* / 1 Liter)

From €12.50*
Anode sleeve fuzzy
Anode pad / tampon / anode sleeve / fuzzy sleeve / replacement fabric pad puffy from Betzmann Galvanik.    This puffy fabric pad / anode sleeve or also called tampon is absolutely recommended for all plating processes. Optimally suitable for all coatings and electrolytes.  The coating of larger areas is also quite fast with this pad.   The insertion hole is larger than the electrode and therefore it happens that the moist  anode pad slips off. Therefore, fix the pad on the electrode with a small rubber band.    

€2.38*
MPU - Metal Polish Ultra
MPU is an excellent preparation compound for brush and tank electroplating as it cleans, polishes and activates all in one stage. It quickly creates a water break free surface on a wide range of metals.   Features Used One stage cleaning and activating product For cleaning and activating in one stage, can replace the ActiClean stage – saves time and money Can be used during the plating process without having to re-electroclean and activate Clearing burns or other marks produced during plating – all you have to do is rinse and carry on plating

Content: 0.1 Liter (€125.00* / 1 Liter)

From €12.50*