Gold Solution 8 Gramm / Liter
€540.00
Available, delivery time: 1-2 days
Product information "Gold Solution 8 Gramm / Liter"
Gold Electrolyte 8 g/L – 24K Hard Gold Plating Solution
Professional Gold Electrolyte for Bath Plating, Pen Plating and Brush Plating
The BMG-067 Gold Electrolyte from Betzmann Galvanik contains 8 g/L of gold and is designed for high-quality electroplating applications.
Its specially formulated composition produces a hard, wear-resistant and uniform gold deposit with a hardness of approximately 220–230 HV.
With a specified gold content of 99.9% in the deposit, this electrolyte is suitable for premium decorative and technical gold plating applications.
The electrolyte can be used for conventional immersion plating as well as selective pen plating and brush plating.
For applications requiring thicker gold coatings, deposits exceeding 10 µm can also be achieved under suitable operating conditions using an appropriate platinum electrode.
Key Features and Benefits
Gold concentration: 8 g/L
Specified gold content in the deposit: 99.9%
24-karat gold plating
Deposit hardness: approximately 220–230 HV
Good wear resistance
Suitable for immersion and bath plating
Suitable for pen plating
Suitable for brush plating
Platinum or carbon/graphite electrodes
Standard maximum deposit thickness according to manufacturer: approximately 5 µm
Deposits exceeding 10 µm possible under suitable conditions
Suitable for decorative and technical applications
Technical Specifications and Operating Conditions
| Parameter | Manufacturer Specification |
|---|---|
| Product number | BMG-067 |
| Gold concentration | 8 g/L |
| Voltage range | 3–5 V |
| Reference voltage | 3.5 V |
| Operating temperature | 14–25 °C |
| Suitable electrodes | Platinum or carbon/graphite |
| Gold content in deposit | 99.9% |
| Remaining deposit component | Carbon |
| Plating rate | Approx. 0.5 µm/min at 3.5 V with platinum electrode (spot plating) |
| Cathodic efficiency | 35–40% at 3.5 V with platinum electrode |
| Maximum standard deposit thickness | Approx. 5 µm |
| Extended deposit thickness | Over 10 µm possible under suitable conditions |
| Deposit hardness | 220–230 HV |
| Deposit density | 19.3 g/cm³ |
| Internal stress | Medium |
| Storage requirements | Protect from direct sunlight |
| Shelf life | 1 year |
| Health and safety classification | Harmful (manufacturer specification) |
| Special ingredients | Contains 0.3% potassium cyanide |
| Transport classification | No UN number; not classified as dangerous goods for transport |
Recommended Current Density and Operating Voltage
The recommended operating voltage range is 3–5 volts. The manufacturer's reference condition for the specified plating rate is 3.5 volts using a platinum electrode.
For immersion bath plating, we recommend starting with a moderate current density and adjusting the operating parameters according to the workpiece geometry and deposit quality.
Suggested starting values for practical trials:
| Application | Current Density |
|---|---|
| Bath plating – starting range | 0.5–1.0 A/dm² |
| Bath plating – extended trial range | 1.0–1.5 A/dm² |
| Pen plating | Depending on electrode and contact area |
| Brush plating | Depending on swab size and contact area |
These current density values are suggested practical trial ranges and are not manufacturer-confirmed operating specifications.
The optimum current density depends on the workpiece surface area, electrode distance, bath movement, temperature and component geometry.
Voltage alone does not determine current density. We therefore recommend using a regulated DC power supply with adjustable current control.
Calculation example:
For a workpiece surface area of 20 cm² and a current density of 0.01 A/cm²:
20 cm² × 0.01 A/cm² = 0.20 A
The current should be monitored and controlled throughout the plating process to achieve consistent coating results.
Suitable Electrodes – Platinum or Graphite?
This gold electrolyte can be used with both platinum and graphite/carbon electrodes.
Platinum Electrode – Our Recommendation
Excellent chemical resistance
Long service life
Suitable for professional electroplating applications
Reference electrode for the manufacturer's specified plating rate
Particularly suitable for thicker gold deposits
For professional applications, especially when aiming for gold deposits exceeding 10 µm, we recommend using a suitable platinum electrode.
Graphite / Carbon Electrode
Economical alternative to platinum
Suitable for compatible electroplating applications
Interesting option for larger electrode surfaces
Suitable for various bath and selective plating applications
Important: We strongly advise against using stainless steel anodes for most of our electroplating processes.
Gold Deposits Exceeding 10 µm
The manufacturer's specified standard maximum deposit thickness is approximately 5 µm.
For applications requiring thicker gold coatings, deposits exceeding 10 µm can also be achieved under suitable process conditions.
For these applications, we recommend using a platinum electrode and carefully controlling the current and other operating parameters.
With increased deposit thickness, particular attention should be paid to uniform deposition, adhesion and electrolyte stability.
The achievable thickness depends on the actual plating setup and must be verified under the intended operating conditions.
Suitable Applications
This 8 g/L gold electrolyte is suitable for:
Jewellery and jewellery components
Watches and watch components
Metal fittings and decorative parts
High-quality decorative objects
Restoration and repair gold plating
Electrical contacts and metal components
Technical surface finishing
Individual and custom plating applications
Workpiece Preparation
The adhesion and quality of the gold deposit depend heavily on proper surface preparation.
Before plating, the workpiece must be thoroughly cleaned, degreased and, where necessary, activated.
Depending on the substrate material, such as stainless steel, copper, brass, silver or steel, a suitable intermediate layer or adhesion treatment may be required.
Proper surface preparation is essential for achieving a durable, uniform and well-adhering gold coating.
Storage and Shelf Life
Store the gold electrolyte protected from direct sunlight.
The manufacturer's specified shelf life is one year when stored under suitable conditions.
Betzmann Galvanik – Your Partner for Professional Electroplating
Betzmann Galvanik supplies high-quality electroplating electrolytes and the corresponding equipment for professional surface finishing.
Our product range includes:
Gold, silver, platinum and rhodium electrolytes
Electroplating equipment and regulated DC power supplies
Graphite and platinum electrodes
Anodes and anode pads
Complete systems for bath plating
Accessories for pen plating and brush plating
Benefit from our many years of experience in electroplating technology and our personal technical support.
Order your 8 g/L Gold Electrolyte now and achieve high-quality 24-karat gold deposits with Betzmann Galvanik.
Pictogram
Signal word Danger
Hazard statement(s)
H302 Harmful if swallowed.
H313 May be harmful in contact with skin.
H317 May cause an allergic skin reaction.
Precautionary statement(s)
P261 Avoid breathing dust/ fume/ gas/ mist/ vapours/spray.
P305 + P351 + P338 IF IN EYES: Rinse cautiously with water for several minutes. Remove contact lenses, if present and easy to do. Continue rinsing.
Precautionary statement(s)
P261 Avoid breathing dust/fume/gas/mist/vapors/spray.
P305 + P351 + P338 IF IN EYES: Rinse cautiously with water for several minutes. Remove contact lenses, if present and easy to do. Continue rinsing.
HS Code: 3824 99 70